Mechanical Properties

Yield Tensile Strength

586 MPa

Ultimate Tensile Strength

862 MPa

Tensile Modulus

200 GPa

Shear Strength

345 MPa

Shear Modulus

76 GPa

Fatigue Strength

359 MPa

Elongation At Break

28 %

Poisson's Ratio

0.30

Hardness

32 HRC

Density

7.8 g/cm³

Impact Strength (ASTM)

110 J/m

Electrical/Magnetic Properties

Surface Resistance (ANSI)

-

Magnetism

Weak

Thermal Properties

Heat Deflection Temperature

300 °C

Thermal Expansion Coefficient

13.0 µm/(m⋅°C

Specific Heat Capacity

0.500 J/g°C

Thermal Conductivity

15 W/(m⋅°C)

Melting Point

1400 °C

Chemical Properties

Corrosion Resistance

Excellent

Super Duplex 2507 (UNS S32750)

High-strength, corrosion-resistant stainless steel

Get your parts manufactured today.

Get Instant Quote

Material Datasheet

Material Type

Metal

Material Sub-Type

Stainless Steel

Material Name

Super Duplex 2507 (UNS S32750)

Note: Properties are not guaranteed. They are intended only as a basis for comparison and not for design purposes.

Mechanical Properties

Yield Tensile Strength

586 MPa

85.0 Ksi

Ultimate Tensile Strength

862 MPa

125.0 Ksi

Tensile Modulus

200 GPa

29.0 Msi

Shear Strength

345 MPa

50.0 Ksi

Shear Modulus

76 GPa

11.0 Msi

Fatigue Strength

359 MPa

52.0 Ksi

Elongation At Break

28 %

-

Poisson's Ratio

0.30

-

Hardness

32 HRC

-

Density

7.8 g/cm³

0.282 lb/in³

Impact Strength (ASTM)

110 J/m

2.06 ft⋅lb/in

Electrical/Magnetic Properties

Surface Resistance (ANSI)

-

-

Magnetism

Weak

-

Thermal Properties

Heat Deflection Temperature

300 °C

572 °F

Thermal Expansion Coefficient

13.0 µm/(m⋅°C

7.2 µin/(in⋅°F)

Specific Heat Capacity

0.500 J/g°C

0.119 BTU/lb-°F

Thermal Conductivity

15 W/(m⋅°C)

8.7 BTU/(h⋅ft⋅°F)

Melting Point

1400 °C

2552 °F

Chemical Properties

Corrosion Resistance

Excellent

-